[* black] |
[* black] |
[* black] Be careful not to allow epoxy to over-flow into the hole of the syringe as this will need to be clear for the syringe plunger (which acts as a pressure relief valve). |
[* black] Make sure to keep for use later. |
[* black] This needs to cure before we can flip it over and do the other side. 3 hours for the Hysol and 8-12 hours for the Devcon. |
[* black] Once it is set, you can get back to testing and hopefully back in the water. |